(1)FILM
Use times: >30 times : plastic pp film faced plywood
Use times: between 5-10 times : brown /black film faced plywood
Use times: 8mm ± 0.5 mm or ± 0.8mm
(2)Glue
MRMelamine/Phnenolic glue
(3)Core
poplar/eucalyptus/combined/hardwood
(4)Hot Press Times
1 time hot press / 2 times hot press
Use times: >30 times : plastic pp film faced plywood
Use times: between 5-10 times : brown /black film faced plywood
Use times: 8mm ± 0.5 mm or ± 0.8mm
(2)Glue
MRMelamine/Phnenolic glue
(3)Core
poplar/eucalyptus/combined/hardwood
(4)Hot Press Times
1 time hot press / 2 times hot press